this post was submitted on 01 Sep 2026
18 points (95.0% liked)

3DPrinting

23695 readers
67 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 3 years ago
MODERATORS
 

I've seen many debates about the need to dry PLA filaments. Looks like some people never need to do anything while others dry the hell out of them before printing.

I've been recommended once to print at 10% RH… After 48h of drying, I can barely get below 37%…

So: what's the humidity level in the room your printer is?

you are viewing a single comment's thread
view the rest of the comments
[–] Bluewing@lemmy.world 2 points 6 days ago

In northern Minnesota the humidity can vary greatly. Last weekend it was 90+% outside. While indoors the air conditioning had the house around 50%. And by winter time, the outdoor humidity can be as low 20% and indoors depending on heat source, around 30% to 40%.

I finally broke down and bought a dedicated filament dryer, Sunlu S2, because my trusty old food dehydrator died the week before. I do dry PETG when it tells me to, and I always dry TPU. But never PLA.

Just for fun, after I was done drying and printing some PETG, I dropped a mostly used spool of Sunlu white PLA into the dryer, (first time ever for PLA). That spool has been laying around in the open for at least 6 months now. The humidistat on the dryer showed 30%. I let it dry down to 20% and ran a test cube. No difference in print quality that I can see.